Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_753c0e36e3801d4916536a65a77efc35 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-547 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-02363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-1804 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-306 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-0236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-18 |
filingDate |
2007-07-12^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-02-26^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_980f17b0370e44a60908a1091bbb8dc2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd886358196fb96635c2782b77973a5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87d70d3f23ec67d3911d955059b007a1 |
publicationDate |
2014-02-26^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-101507000-B |
titleOfInvention |
Method of texturing silicon wafer for fabricating solar cells |
abstract |
The present invention discloses a method for producing solar battery for texturing the silicon wafer. In the method, a step of introducing silicon wafer relates to adopting a texturing processing solution. The temperature of texturing processing solution is at least 80 DEG C. The texturing processing solution comprises water which is combined with 1%-6% of KOH by weight or 2%-8% of NaOH by weight, and less than 0.01% of surfactant or surfactant compound by weight. The economical texturing processing can be executed with the mode. |