http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103357510-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8ec5284b467459bc08e01a5e2e123638 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-018 |
filingDate | 2013-07-26^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-24^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b17f45306c428af998bb1d4a2441a71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7d545eaffeb5e91c56f1a5e261a6033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_84930a35474a4e769d74e83fef3eb4cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_403342c2a841fbfe5d50cb6bc6ff5c6b |
publicationDate | 2014-12-24^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103357510-B |
titleOfInvention | Cellophane positive flotation collector and preparation method of cellophane positive flotation collector |
abstract | The invention relates to a cellophane positive flotation collector and a preparation method of the cellophane positive flotation collector, in particular to a cellophane positive flotation collector compounded by fatty acid and the like, wherein the basic substances comprise the following preparation raw materials in percentage by weight: 30 to 80 percent of chlorinated oleic acid, 5 percent to 60 percent of saturated higher aliphatic acid, 5 percent to 40 percent of unsaturated higher aliphatic acid and 5 percent to 20 percent of alkali, the saturated higher aliphatic acid is one of materials from tetradecanoic acid, stearic acid and palmitic acid, and the unsaturated higher aliphatic acid is one of materials from oleic acid, coconut oil and linoleic acid. By aiming at the Yunnan phosphorite characteristic, the positive flotation collector has high selectivity and high mine carrying capability, the better sorting effect is realized at the normal temperature, and excellent flotation indexes can be reached. By aiming at the refractory cellophane, the comprehensive mineral dressing efficiency and the recovery rate of phosphate concentrate after the flotation are higher. |
priorityDate | 2013-07-26^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 42 of 42.