http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105344495-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2203-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-018 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D103-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-018 |
filingDate | 2015-11-30^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-07-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-07-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105344495-B |
titleOfInvention | A kind of method that zinc oxide is reclaimed in the flotation tailing from zinc sulphide |
abstract | A kind of method that zinc oxide is reclaimed in flotation tailing from zinc sulphide, comprises the following steps:(1) high alkalinity zinc sulphide flotation tailing is concentrated into 45wt%, adds 800g/t 1200g/ citric acids, stirring reaction 10 15 minutes.(2) 3kg/t of vulcanized sodium 2 is added, then stirring reaction 5 minutes adds clear water, by concentration dilution to 30wt%.(3) 500g/t of primary octadecylamine acetate 300, stirring reaction 5 minutes are added;(4) No. 2 160g/t of oil 120 are added, stirring reaction is after 3 minutes, and now pH values of pulp is 8.5 9.5.Start inflation and scrape bubble flotation, you can obtain high-quality zinc oxide product. |