http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106380990-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2305-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2443-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F230-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-0427 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L31-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L31-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F216-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L31-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L31-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L31-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F230-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-34 |
filingDate | 2016-08-27^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-05-11^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-05-11^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106380990-B |
titleOfInvention | The preparation method of phosphoryl choline polymer containing aldehyde radical and dopamine cross-linked coating |
abstract | The invention discloses the preparation method of a kind of phosphoryl choline polymer containing aldehyde radical and dopamine cross-linked coating, including:First, the phosphoryl choline polymer containing aldehyde radical is prepared;2nd, dopamine and phosphoryl choline polymer containing aldehyde radical are dissolved in polar solvent and obtain mixed solution, the mixed solution is then coated on material surface to be modified, is dried;3rd, the material to be modified after drying is placed in alkaline aqueous solution, heats 2h~12h under the conditions of 40 DEG C~90 DEG C, obtains the crosslinking adhesion bionic coating with imitating cell outer-layer membrane structure.The preparation method of the present invention is simple and convenient to operate, the crosslinking adhesion bionic coating surface with imitating cell outer-layer membrane structure to obtain stable provides a kind of new approach, the coating of preparation will be in blood purification, it is material implanted, the fields such as organizational project, medicament slow release and biology sensor have broad application prospects. |