http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106733208-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2203-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-007 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03B1-00 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D103-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03B1-00 |
filingDate | 2017-01-11^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-11-20^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-11-20^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106733208-B |
titleOfInvention | Low ash divides semi-coke and its wet flotation technique |
abstract | The invention discloses a kind of low ashes to divide semi-coke and its wet flotation technique, and the wet flotation technique of the low ash point semi-coke includes the following steps:(1) semi-coke is crushed, crosses 32 meshes;(2) semi-coke for crossing 32 meshes is mixed with water, obtains ore pulp, adjusting pulp density is 50-80g/L;(3) ore pulp is subjected to ultrasonic treatment 5-15min, ultrasonic treatment carries out in three stages;(4) flotation device is added in the ore pulp after ultrasound, then surface modifier is added into flotation device;(5) kerosene is added as collecting agent;(6) secondary enanthol is added as foaming agent;(7) it inflates;(8) it filters, dry, obtain low ash point semi-coke.Low ash of the present invention divides semi-coke and its wet flotation technique, has carried out Study of deashing to semi-coke using the method for froth flotation, has investigated the optimum process condition of semi-coke flotation;Influence of some factors to grey rate is dropped has been investigated with the method for orthogonal experiment;To being ultrasonically treated before semi-coke flotation, its influence to flotation effect is probed into;Dosing is reduced, flotation effect is improved. |
priorityDate | 2017-01-11^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |