http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110564106-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-06 |
filingDate | 2019-09-06^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-03-22^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-03-22^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110564106-B |
titleOfInvention | High-strength synthetic resin for glass fiber rod and preparation method thereof |
abstract | The invention discloses a high-strength synthetic resin for a glass fiber rod and a preparation method thereof, belonging to the technical field of synthetic resin products. According to the invention, the cation exchange performance of the sodium bentonite is utilized, cations in the superfine silicon dioxide and the alumina are exchanged and enter the bentonite layer, and then the plasma sputtering is used for carrying out pore forming on the bentonite layer to obtain the plasma modified sodium bentonite, so that the adsorbability of the bentonite is improved, the sodium bentonite also has aging resistance, the high temperature resistance and the mechanical strength of the synthetic resin can be increased, and the high water absorption of the resin can be kept to the maximum extent; the fluidized coating layer material is coated outside the microporous coating reinforcing agent, so that the mechanical strength of the microporous coating reinforcing agent is improved, and the mechanical strength of the obtained synthetic resin is obviously enhanced. |