http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112452549-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2203-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D2201-007 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03D1-018 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D103-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-018 |
filingDate | 2020-10-22^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-03-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-03-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112452549-B |
titleOfInvention | Beneficiation method for micro-fine particle tungsten ore |
abstract | The invention provides a beneficiation method of micro-fine tungsten ore, belonging to the technical field of beneficiation. Firstly, grinding tungsten ore, then adding a mixture of regulator sodium carbonate, inhibitor sodium alginate and collector 731 oxidized paraffin soap and polyether to stir and size, and roughly selecting tungsten by using a flotation machine to obtain roughly selected concentrate and roughly selected tailings; adding sodium alginate into the roughed concentrate, carrying out five-time concentration to obtain concentrate 1, adding a mixture of 731 oxidized paraffin soap and polyether into the roughed tailings, carrying out scavenging twice, obtaining scavenged tailings, adding a regulator acidified water glass and a collector poly (N-isopropylacrylamide) into the scavenged tailings, carrying out flotation by using a flotation column, obtaining concentrate 2 and final tailings, and combining the concentrate 1 and the concentrate 2 into final concentrate. The method solves the technical problem that the micro-fine tungsten ore is difficult to effectively recover, and has important significance for realizing the high-efficiency utilization of the low-grade tungsten ore which is difficult to treat. |
priorityDate | 2020-10-22^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 35 of 35.