Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_535c220dbfca5aee91887c5a6f4fe721 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2009-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C70-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-561 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-34 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-56 |
filingDate |
1991-03-15^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c889c2d0be9dcedfa49c84839778fab3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f06129d511583cc0e06e2989a452c60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c03a5d655820a1c1c9d28e55fe11c279 |
publicationDate |
1991-09-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0446941-A2 |
titleOfInvention |
Method of forming composite moldings and die for carrying out the method |
abstract |
This invention is a method of manufacturing composite moldings by executing the following steps (a) to (f) by using an injection modling machine provided with a fixed die (12) having a gate which is opened to a cavity forming surface and a movable die (13) which can be come into contact with and removed from the fixed die:n (a) step of setting a desired skin material (18) to a predetermined position of the movable die (13) in a state in which the movable die was sufficiently removed from the fixed die (12); (b) a first die clamping step in which the movable die (13) is moved toward the fixed die (12) and is stopped at a position where an interval (T) between the movable and fixed dies is equal to a predetermined value of 5 mm or more; (c) step of injecting a fused resin into a cavity; (d) a second die clamping step in which the movable die (13) is stopped at a desired last position; (e) step of cooling for a predetermined time after the second die clamping step; (f) step of removing the movable die from the fixed die and opening the dies and taking out a product. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1982817-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6596218-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19505155-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0016958-A1 |
priorityDate |
1990-03-15^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |