abstract |
Thermoplastic elastomers with good dyeability and high strength and elasticity, whose embedded elastomer particles have an average particle diameter of 0.05 to 5 µm, are formed by a process in which mixtures of propylene homopolymers and / or propylene copolymers, elastomeric C 4 -C 12- olefin co- and / or terpolymers and C 8 -C 14 diacrylates, C 7 -C 16 diallyl compounds, C 9 -C 15 dimethacrylates, C 7 -C 10 divinyl compounds, C 12 -C 17 - Acrylic acid esters of polyalcohols, C 15 -C 21 methacrylic acid esters of polyalcohols and / or C 9 - C 12 triallyl compounds are reacted in the melt.n n n The thermoplastic elastomers and blends with conventional polyolefins arenfor use in the automotive industry, household appliance industry, on thenSuitable for the construction sector and in medical technology. |