Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b502fde933db1d6126d10bbcbddb83ea |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-78 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-07 |
filingDate |
2002-01-08^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02c3a351ee5e2dc0e6ec79da31ee7515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_70d5f8b2c399e31612361ae74f2d4433 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_331d49c1b9fbd31b1b6287b1ec6d69f1 |
publicationDate |
2003-12-10^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1368508-A1 |
titleOfInvention |
Aqueous surface conditioner and surface conditioning method for phosphating treatment |
abstract |
An aqueous surface conditioner for use in a phosphating treatment is provided which contains crystals having an average diameter of 5 νm or less in an amount of at least 0.1 g/L. The crystals are selected to have a two-dimensional epitaxy that matches within 3 % of misfit with the crystal lattice of one phosphate coating selected from among (1) hopeite /Zn3(PO4)2.4H2O) and/or phosphophyllite (Zn2Fe(PO4)2.4H2O), (2) scholzite (CaZn2(PO4)2.2H2O) and (3) hureaulite (Mn5(PO4)2[PO3(OH]2.4H2O). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012126734-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2503025-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9534301-B2 |
priorityDate |
2001-01-09^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |