abstract |
A method for producing a laminate (E) of a low air permeable resin/rubber composition comprising: nlaminating a laminate (D) of a low air permeable resin (A) layer having an air permeation coefficient of 1.0×10 -12 cc·cm/cm 2 ·sec·cmHg or less and an average thickness d (µm) of 0.05<d<5 and a thermoplastic resin composition (B) layer with a rubber composition (E) layer so as to form (B)/(A)/(E), followed by vulcanization, and npeeling off only the thermoplastic resin composition (B) from the laminate, as well as the laminate thereof. |