http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2351791-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ef42db06e1962e22b67cc240173d8ea |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C1-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 |
filingDate | 2009-11-26^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6780c4999367040fefb21ba0544c7ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53b2fa804f5b79c0ec02858886f0e503 |
publicationDate | 2011-08-03^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2351791-A1 |
titleOfInvention | Resin composition for plating use and resin plated product |
abstract | There is provided a resin composition for plating use in which all of plating adhesion strength, moldability, impact resistance, and low coefficient of linear expansion are excellent; and a resin plated product. n The resin composition for plating use of the present invention is characterized by including a graft copolymer (A) formed by graft polymerizing a specific monomer component onto a rubber-like polymer (d) constituted of a conjugated diene-based rubber, and a specific copolymer (B), wherein a proportion of the rubber-like polymer (d) is 10 to 20% by mass, relative to the combined total of the graft copolymer (A) and the copolymer (B) which accounts for 100% by mass, and also 1 to 8 parts by mass of an antioxidant (C) having a melting point of 25 to 100°C is added, relative to the combined total of the graft copolymer (A) and the copolymer (B) which accounts for 100 parts by mass. |
priorityDate | 2008-11-27^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 289 of 289.