http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2634161-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27D2019-0015
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6583
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6584
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6562
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6567
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6565
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27D19-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27D17-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-64
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D99-0089
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-638
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B5-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B5-16
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27B5-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D17-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-64
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-638
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27B5-14
filingDate 2011-10-25^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3e2c67a29699e39cf77a643619e3c33
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fa5ffbc11106ad880b406a062aa7fe39
publicationDate 2013-09-04^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-2634161-A1
titleOfInvention Method for producing fired body and firing furnace used therefor
abstract The method for producing a fired body of the invention has the steps of: preparing a starting material that is a mixture containing an inorganic compound, an organic binder and a solvent; molding the mixture to obtain a green molded body; a first heating step to make the molded body contain residual carbon-containing substances in a furnace by increasing the temperature of the furnace while introducing a gas with an oxygen concentration of 1 to 5 vol%; and a second heating step following the first heating step to obtain a fired body by further increasing the temperature of the furnace without introducing the gas with an oxygen concentration of 1 to 5 vol%; wherein the conditions for the first heating step are set so that when the molded body is allowed to stand after the first heating step in an oxygen-containing atmosphere at 900°C, the temperature at the center section of the molded body is at least 20°C higher than the temperature of the atmosphere in the furnace.
priorityDate 2010-10-29^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425534311
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID129488327
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID977
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID16213786
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID426223290
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10467
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419523291
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID51240
http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID51240
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581

Showing number of triples: 1 to 39 of 39.