http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2712849-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8601904b5a87e2ab79561ccf035ffa24 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C4-0092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-087 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C4-00 |
filingDate | 2013-09-26^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e4a8ea2c52617fd40dea0690c63e8a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb1b618903bbc4819ee412b8a4c185d8 |
publicationDate | 2014-04-02^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2712849-A1 |
titleOfInvention | A flat glass application with low iron content |
abstract | A 2-12 mm flat glass consisting of components with below percentages per weightn nis characterized in that in order for said flat glass to have a daylight transmittance of minimum 90 ± 1 %, a solar energy transmittance of minimum 87 ± 1 % and a redox ratio of iron ≤ 0.25; the Fe +2 ions, arising from Fe 2 O 3 in said flat glass batch, is at a maximum value of 0.006% in weight and said flat glass includes the below mentioned component percentages by weight for the iron inside said batch to be oxidized and passivated: |
priorityDate | 2012-09-28^^<http://www.w3.org/2001/XMLSchema#date> |