Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_01c1e0bc0628f76dea731cda5a666ca1 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate |
1999-11-12^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb0ae760caed2238b80c7cde3090634a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_472e391ea55b581bef37d53633d10190 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf24f8edc682effc6bae84df7718bde0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e441505629ffe2dcaa041e4211b2ba80 |
publicationDate |
2001-05-22^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2001139790-A |
titleOfInvention |
Flame retardant thermoplastic resin composition |
abstract |
(57) Abstract: Flame retardant thermoplastic resin composition having excellent flame retardancy and chemical resistance by blending a polycarbonate resin and a polyester resin, and a specific polyorganosilsesquioxane compound. I will provide a. SOLUTION: (A) a polycarbonate resin and (B) a thermoplastic polyester resin are mixed with 95/5 to 60 / 100 parts by weight of a resin contained in a weight ratio of 40, and (C) a specific polyorganosilsesquioxane compound of 0.5 to 2 A flame-retardant resin composition containing 0 parts by weight is used. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1288262-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100853142-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005103154-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-1330705-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005103154-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009091533-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6727303-B2 |
priorityDate |
1999-11-12^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |