http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002541289-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L19-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-20 |
filingDate | 2000-03-20^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2002-12-03^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002541289-A |
titleOfInvention | Hydroxyl group-containing rubber mixture |
abstract | (57) [Summary]nThe present invention relates to a rubber mixture comprising a rubber polymerized in a solution having a secondary hydroxyl group content of from 0.1 to 5% by weight, whose groups are located within 4 carbon atoms from each side chain end. About. The invention also relates to mixtures of the rubber mixtures with fillers, optionally further rubbers and rubber auxiliaries, and vulcanized rubbers produced therefrom. The rubber mixtures according to the invention are useful for the production of high-strength abrasion-resistant moldings, in particular for the production of tires characterized by excellent non-skid properties on wet surfaces. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012528213-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012505943-A |
priorityDate | 1999-04-01^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 136 of 136.