http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004204005-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 |
filingDate | 2002-12-25^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_db22a0ce6b58547e9ce1b5e15a9baa89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6313c9d4ba910ed2c7eef122262c435a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1dd93650925852d0fcf43058982c2a6c |
publicationDate | 2004-07-22^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004204005-A |
titleOfInvention | Aromatic polycarbonate resin composition |
abstract | The present invention provides an aromatic polycarbonate resin composition having good rigidity, heat stability and moldability. (A) 100 parts by weight of an aromatic polycarbonate (A component), (B) 0.1 to 50 parts by weight of a layered silicate (B component) having a cation exchange capacity of 50 to 200 meq / 100 g, And (C) a compound having an affinity for the aromatic polycarbonate (Component A) and having a hydrophilic component (Component C) in an amount of 0.1 to 50 parts by weight. Melt volume rate MVR (cm 3 / cm 3) measured at 250 ° C. under a load of 2.16 kg with a composition comprising 0.005 to 1 part by weight of a partial ester and / or full ester (component D) of a polyhydric alcohol 10 min) and a viscosity average molecular weight Mv satisfying the following formula (I). MVR + (Mv × 0.003)> 65 (I) [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011030800-A |
priorityDate | 2002-12-25^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 369 of 369.