http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005048176-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-22 |
filingDate | 2004-07-14^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e71b361e982e944c4638f54519b022c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_557f0d6dabee6644a2284c97e2904033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a15b4b69bffe83847f6ba0b4908fc38e |
publicationDate | 2005-02-24^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005048176-A |
titleOfInvention | Resin particles and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide excellent concealability when used as an additive for paints or cosmetics, and to maintain ink when used as an additive for paper coating, and to be abrasive when used with an abrasive. To obtain resin particles excellent in. A resin particle comprising a resin (a) and a filler (b) [wherein the particle has a volume average particle size of 0.1 to 300 μm and a shape factor (SF-2) of 110 to 300. The particles have an outer shell layer (S) comprising at least a part of (b); the layer (S) is at least 0.01 μm and less than or equal to ½ of the maximum inscribed circle radius of the particle cross section Has a thickness]. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10007203-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009179756-A |
priorityDate | 2003-07-14^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 844 of 844.