http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005169815-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b5d58119b48e6e6ae449afc394066f3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2003-12-10^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0c7d6a83df28e619961da7478b32b27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b18352553fa28de7c9b1f1bfadc5b5e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a083f01d74a8451d327e445037b68a0 |
publicationDate | 2005-06-30^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005169815-A |
titleOfInvention | Laminated plate |
abstract | PROBLEM TO BE SOLVED: To provide a plate mainly composed of a lactic acid resin having excellent transparency, heat resistance and impact resistance. SOLUTION: A sheet made of a lactic acid resin (A) having a D-form ratio of less than 6% and stretched by 2 to 16 times in an area magnification, and a D-lactic acid resin having a D-form ratio of 6% or more. By producing a plate formed by laminating sheets made of (B), the haze at 3 mm thickness based on JIS K 7105 is 50% or less, the deflection temperature under load based on JIS K 7191 is 60 ° C. or higher, and JIS K 7110 A plate having an Izod impact strength based on 5 kJ / m 2 or more can be obtained. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007026489-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8431212-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008179140-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5162900-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007026489-A1 |
priorityDate | 2003-12-10^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 115 of 115.