http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005227443-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14df928cce1112b89356928855b60351 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 |
filingDate | 2004-02-12^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a764910a675af3e31d75f38e4442686b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b9fd4094050d5e13ec9ea4d211af332 |
publicationDate | 2005-08-25^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005227443-A |
titleOfInvention | Antireflection film, polarizing plate and liquid crystal display device |
abstract | PROBLEM TO BE SOLVED: To achieve surface hardness, scratch resistance and adhesion even in a harsh environment such as high temperature and high humidity without surface unevenness, high surface hardness, scratch resistance and high adhesion to a substrate. Is to provide an antireflection film, a polarizing plate and a liquid crystal display device which do not fluctuate and are excellent in alkali resistance. An antireflection film comprising a low refractive index layer laminated on a layer containing metal oxide fine particles and having a surface centerline average surface roughness Ra of 3 to 20 nm. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015225785-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112672878-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112672878-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115038763-A |
priorityDate | 2004-02-12^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 386 of 386.