http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011153300-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 2010-12-27^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9cf2d31223ba00943ece7dfb190f5483 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b728de7ab8fef617c05f0899f59cff9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2f6c5206689c8caa564d084e2a7ad4b |
publicationDate | 2011-08-11^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011153300-A |
titleOfInvention | Resin composition for molded article for conveyor |
abstract | PROBLEM TO BE SOLVED: To provide a molded article for a conveying material that does not impair the excellent mechanical properties and good appearance of a thermoplastic resin molded article and has sufficient permanent antistatic properties even when the content of the antistatic agent is smaller than that of the conventional one. Provided is a resin composition for a molded article for a conveying material. SOLUTION: An antistatic agent (A) and a thermoplastic resin (B) are contained, the melt viscosity ratio at 220 ° C. of (B) and (A) is 0.5 to 5, and the difference in solubility parameter is A resin composition for a molded article for a conveying material having an absolute value of 1.0 to 3.0, and a molded article for a conveying material formed by molding the composition. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013091777-A |
priorityDate | 2009-12-29^^<http://www.w3.org/2001/XMLSchema#date> |