http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011213021-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-12 |
filingDate | 2010-03-31^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f8599f54bda232a591ae9753c3d60f5 |
publicationDate | 2011-10-27^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011213021-A |
titleOfInvention | Pre-coated aluminum plate for molding and molded container |
abstract | [PROBLEMS] To provide a precoated aluminum plate for molding having a metallic appearance having excellent formability, heat dissipation and brightness. A molding pre-coated Al plate 1 comprising a first coating 3 formed on one side of an aluminum (Al) plate 2 and a second coating 6 formed on the other side of the Al plate 2, The first film 3 includes a crosslinked polyester resin 4 obtained by crosslinking a polyester resin having a Tg of 25 to 100 ° C. with a melamine curing agent or an isocyanate curing agent, and a metallic pigment 5, and has a wavelength of 3 to 30 μm. The infrared integral emissivity is 0.6 or more at a temperature of 25 ° C., the gel fraction is 50% or more, and the second coating 6 is a polyester resin having a Tg of 0 to 80 ° C. as a melamine curing agent or isocyanate curing agent. Incorporated cross-linked polyester resin 7 and additive 8 are used, and the integrated emissivity of infrared rays having a wavelength of 3 to 30 μm is 0.6 or more at a temperature of 25 ° C., and the gel fraction is 50% or more. . [Selection] Figure 1 |