http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011216156-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-702 |
filingDate | 2010-03-31^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_acd15688f03e7c04a265f9773c8bd0e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd5b84d3b2b0d513fb15bf4a30054186 |
publicationDate | 2011-10-27^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011216156-A |
titleOfInvention | Binder for magnetic recording medium, magnetic recording medium, and novel polyurethane resin |
abstract | A magnetic recording medium suitable for high-density recording, in which various powders are highly dispersed. A binder for a magnetic recording medium, which is a polyurethane resin having a cyclic acetal structure represented by the following general formula (I) and an ionic polar group. [In General Formula (I), R 1 and R 2 each independently represent a hydrogen atom or an alkyl group, or are linked to each other to form a ring structure. R 3 to R 6 each have at least one bonding site with the main chain of the polyurethane resin, or have a bonding site in a ring structure formed by linking two or more, and the others are each independently hydrogen. An atom, an alkyl group, or an alkoxyl group is represented. ] [Selection figure] None |
priorityDate | 2010-03-31^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links