http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014069494-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_89afae566b725ae78e20cf972d9bcdc7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-00 |
filingDate | 2012-09-28^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_befcbb548d7ab004fd7506ac4a3fe6be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dacf64c8c75c97980faa28656244e38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_30a2cc4e6f198436bc96dad83de08a26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3013e2b7cd1af4620bdb275103f57d3e |
publicationDate | 2014-04-21^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014069494-A |
titleOfInvention | LAMINATE MANUFACTURING METHOD AND LAMINATE |
abstract | A laminate having excellent chemical resistance and a method for producing the same are provided. A substrate 11, a light-transmitting support 12 having a hydrophilic surface and supporting the substrate 11, and a substrate 11 provided between the support 11 and irradiated through the support 12. After the surface treatment process in which the manufacturing method of the laminated body 1 provided with the separation layer 15 that is altered by absorbing light is made hydrophobic at least on the surface of the support 12 on which the separation layer 15 is provided, And a separation layer forming step of forming the separation layer 15 on the hydrophobicized surface. [Selection] Figure 1 |