Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-97 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-32245 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-73265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48247 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-48 |
filingDate |
2015-08-18^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_556b020014493f2742249b946ab81bfb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f76ed5b52a4a67c1897ffbef5e811a4e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32477aa4f5a41021f98fa0f681040e34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b44e4fbb1966ebaecce60b34392af78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad919e120d7c9bca8ba8e8f0f6687963 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3e4a4ced9d80bafd6d00af333a295b8 |
publicationDate |
2016-07-14^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2016128250-A |
titleOfInvention |
Method for producing composite |
abstract |
Disclosed is a method for producing a composite capable of reducing distortion of the composite due to electron beam irradiation. A method for producing a composite includes a step of irradiating a composite R including a metal portion and an electron beam cross-linked resin with an electron beam EB and curing the electron beam cross-linked resin. Irradiate the electron beam EB so that the temperature of the electron beam cross-linking resin is equal to or higher than the glass transition temperature of the resin material included in the electron beam cross-linking resin and lower than the boiling point of the low-boiling point material included in the electron beam cross-linking resin. It is characterized by this. [Selection] Figure 10 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190052645-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102546064-B1 |
priorityDate |
2014-09-10^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |