http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06272117-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_68728377a3fdee771343dccc806f9f8a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-145 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10C3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10C3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10C3-10 |
filingDate | 1993-03-19^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_036d01f07a1af35cdf949ab7c8473300 |
publicationDate | 1994-09-27^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06272117-A |
titleOfInvention | Method for producing activated carbon fiber |
abstract | (57) [Summary] [Objective] To provide an activated carbon fiber having a large specific surface area and a high fiber strength comparable to those obtained from an optically isotropic pitch. [Structure] In an optically isotropic pitch obtained by heat-treating a molten mixture of an optically isotropic pitch that is hard to be anisotropy and an optically isotropic pitch that is easily anisotropy by heat treatment. The optically anisotropic component is 5 to 30 based on the total weight of the pitch. Softening point 220-29 uniformly dispersed at a weight percentage Activated carbon fibers are produced by spinning pitch for spinning at 0 ° C. to prepare pitch fibers, then infusibilizing and then performing activation treatment. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103352276-A |
priorityDate | 1993-03-19^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 22 of 22.