http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H067948-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_208a4193aa7395066c970e082f9fcebc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6402b23ab8782152be47b3996e48a4a |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K101-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K11-08 |
filingDate | 1992-06-12^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3962e7b01af42fe7960a49d85043d83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fdd40adf512d6f2d6e47de4becdd67e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b2a8bfafe5d788a09a58530574fa743 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a841c6eef1212d061bb978faa8104a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1118ad4fadaecce50cec842ee6632d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59242737efa3445c47ccb37bc72c0718 |
publicationDate | 1994-01-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H067948-A |
titleOfInvention | Can barrel manufacturing method |
abstract | (57) [Summary] [Structure] A steel sheet shear-formed so that two facing sides are substantially parallel to each other is deformed into a cylindrical shape with the two parallel sides facing each other, and the two overlapped sides are welded. In the method for manufacturing a welded can body by which a can body is formed, the carbon content of the steel sheet is 0.20% by weight or less, and the basis weight of the steel sheet is 300. mg / m 2 provided the following metal chromium layer and further thereon is provided a 30 mg / m 2 or less of hydrated chromium oxide layer as metal chromium amount in terms, and one surface of the metal Cr of at least the steel plate The layer is deposited in a granular form, and the existence density of the metal Cr particles is 10 10 for the metal Cr particles having a base diameter of 10 nm or more. ~ 10 15 pieces / m 2 and welding speed V (Mpm), welding power supply frequency F (Hz), plate thickness t (m A method for producing a can body, characterized in that welding is performed without mechanically grinding the welded portion under the condition that m) satisfies the following expression (1). 0.96 ≧ V / t · F (1) [Effect] According to the method of the present invention, the can-making environment and the contents of the can are not contaminated by the scattering of the grinding powder, and the adhesion of the coating film on the welding repair coating part is eliminated. And a highly reliable can barrel can be manufactured. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107206539-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107206539-A |
priorityDate | 1992-06-12^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 30 of 30.