abstract |
(57) 【Abstract】 PROBLEM TO BE SOLVED: Industrially, it has breathability, moisture permeability, and water resistance, and further has good texture and high strength (tear strength and tensile yield point strength). To provide a porous sheet excellent in productivity that can be continuously produced safely and at high speed, and an absorbent article using the same. A crystalline polyolefin resin (60 to 90 parts by weight), a volatilization temperature at atmospheric pressure of 240 ° C. or higher, and a melting point of 1 A sheet formed from a melt-kneaded product of a resin composition containing 40 to 10 parts by weight of a compound at 00 ° C. or less is stretched at a stretching ratio of 3 to 30% in the CD direction and a stretching ratio of 20 to 90% in the MD direction. A porous sheet and an absorbent article using the porous sheet. |