http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10287739-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K467-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-66 |
filingDate | 1997-04-15^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24d38f1bd21289dc20c1197678e29462 |
publicationDate | 1998-10-27^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10287739-A |
titleOfInvention | Antistatic polyetherester and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To specify the composition, viscosity and carboxyl group content of a polyetherester for the purpose of imparting antistatic performance, improving durability and stabilizing heat and light. SOLUTION: The number average molecular weight is 400 to 200 in the molecule. A polyether component comprising 20 to 65% by weight of a polyoxyalkylene glycol segment having a relative viscosity of 1.5 to 4.0 as measured in m-cresol at 30 ° C. Having a carboxyl group content of 0.1 to 15 * 10 -6 eq / g polyetherester and its production method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001233950-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03050160-A1 |
priorityDate | 1997-04-15^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 99 of 99.