http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S60195127-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ba60be3b3f99c87e117c7f7c20b7071 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-00 |
filingDate | 1984-03-19^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9c59df77b6a79e02c8eabc38fdbac9a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_204013608f44e09a68206d2aa1494b13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3cd9f20f17a97c52a4286f282e6da77b |
publicationDate | 1985-10-03^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S60195127-A |
titleOfInvention | Curable resin composition |
abstract | PURPOSE: To obtain a composition of outstanding long-term storage stability capable of giving tough cured products through readily curing by light or organic peroxide, by incorporating polythiol in a blend of diallylidene pentaerythrit and oligo(meth)acrylate. n CONSTITUTION: The objective composition can be obtained by incorporating a blend of (A) diallylidene pentaerythrit and (B) origo(meth)acrylate with a molecular weight ≥300, having in one molecule at least two (meth)acryloyl groups with (C) a polythiol in such an amount as to correspond to 0.1W1.5 equivalent of the thiol group per equivalent of the unsaturated bond in said blend. The component (B) is, e.g. a vinyl ester, urethane-acrylate resin. The component (C) is e.g. a pentaerythrit tetrathioglycolate. n COPYRIGHT: (C)1985,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-8702681-A1 |
priorityDate | 1984-03-19^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 73 of 73.