http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007145338-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16J15-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 |
filingDate | 2007-06-15^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-11-12^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007145338-A1 |
titleOfInvention | Acrylic rubber composition |
abstract | An acrylic rubber composition that improves compression set, significantly improves product function, suppresses oil leakage in the cycle test, and suppresses rubber curing deterioration in the curing deterioration test. To provide. (A) For 100 parts by weight of an acrylic rubber polymer obtained by polymerizing a main monomer comprising an alkoxyalkyl acrylate, butyl acrylate, and a crosslinking point monomer having a functional group, (B) iodine adsorption amount 15 to 25 mg / g, a carbon black from 40 to 100 parts by weight of DBP oil absorption 120~130cm 3 / 100g, acrylic rubber composition obtained by blending the (C) 10 parts by weight or less plasticizer. [Selection figure] None |
priorityDate | 2006-06-16^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |