abstract |
The composite fine particles contain an inorganic fine particle and an organic polymer bonded to the surface of the inorganic fine particle, and have an average particle diameter of 5-200 nm and a particle diameter variation coefficient of 50% or less. Such multiparticulates can be obtained by hydrolyzing and condensing an organic polymer, wherein the organic polymer has a polysiloxane group containing at least one Si-OR 1 group per molecule, where R 1 is a hydrogen atom, unsubstituted An unsubstituted or substituted alkyl group or an unsubstituted or substituted acyl group. Dispersions of multiparticulates include multiparticulates and a dispersion medium. The film forming composition contains such a dispersion. |