http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100697754-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-844 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-8428 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K59-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-8423 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K59-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K59-179 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-26 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-52 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J63-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J1-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-12 |
filingDate | 1999-09-22^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-03-21^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-03-21^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100697754-B1 |
titleOfInvention | Optical element and manufacturing method thereof |
abstract | The present invention improves the formation of a laminate including an organic layer, wherein the image panel can be disposed on the display adjacent to the image panel without a gap therebetween, without damaging the surface of the organic layer already formed by the deposition mask. The optical element used as the image panel made into the above, and the manufacturing method of this optical element are disclosed. The metal bumps are provided in the form of stripes of transparent electrodes disposed on the glass substrate so as to be located in the non-optical operating region and are drawn on the back side of the organic EL element. The metal bumps serve as spacers in the deposition of an organic layer or the like to prevent contact between the vapor deposition mask and the vapor deposition mask, and are led out on the back of the organic EL element together with the metal electrode, and are mounted on the back of the organic EL element. Connected with.n n n n Image panel, metal bumps, organic EL element, deposition mask, ready film surface, transparent electrode, non-pixel region, organic layer |
priorityDate | 1998-09-25^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |