http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101527522-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1bc8d5b80410c3a0594da023cfabcbe0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82B3-0095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82B3-00 |
filingDate | 2014-01-16^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-06-18^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef5c9940ac4e7e3dd108c0d09da5e22d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72ebb88393bad227b062da4e5964b24c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c9d5a852fb486ae6a974322fc23af51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d78fec2995fc3d35e1df19ca929511d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5dc4c0eb0ddb1a0861336d0bf93b4d1 |
publicationDate | 2015-06-18^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101527522-B1 |
titleOfInvention | Manufacturing method of silver nano ring and thereof silver nano ring |
abstract | In the present invention, a linear silver nanowire applied as a conductive material of a transparent conductive film is formed into a curved silver nanowire, and then a curved silver nanowire is grown into a circular silver nano-ring By increasing the number of contact points where silver nano rings are overlapped with each other, it is possible to increase the number of contacts that can form a conductive network per unit area of silver nano rings, thereby realizing the same resistance zone in a relatively small amount, Accordingly, the present invention provides a method for producing a silver nanoparticle capable of improving the optical characteristics of a transparent conductive film, and a silver nanoparticle according to the method, and the technical structure thereof includes: heating a reducing solvent; Adding a capping agent to the reducing solvent; Adding a catalyst to the reducing solvent; Adding silver nitrate to the reducing solvent; Heating the reducing solvent to form linear silver nanowires; Heating the reducing solvent at a temperature of 180 ° C or more for 30 minutes or longer to form curved silver nanowires; And adjusting the reaction time of the solvent to grow silver nano-rings; And a control unit. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110524005-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111545768-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110976909-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018029225-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101936118-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3281723-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108436098-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108436098-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110524005-A |
priorityDate | 2014-01-16^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Showing number of triples: 1 to 50 of 50.