http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101684874-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2200-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2505-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2505-022 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-507 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-21 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-507 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-53 |
filingDate | 2010-12-23^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-12-21^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-12-21^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101684874-B1 |
titleOfInvention | Polyketone Fiber with Improved Wearing Property and Method for Preparing the Same |
abstract | More particularly, the present invention relates to a polyketone fiber having improved abrasiveness and a method for producing the polyketone fiber by dissolving a polyketone containing, as a repeating unit, at least 90 mol% of a ketone unit in an aqueous solution of resorcinol. Extruding and radiating the polyketone solution through a spinning nozzle, allowing the polyketone solution to pass through an air layer to reach a coagulation bath, and then solidifying the polyketone solution to obtain a multifilament; And then solidifying to obtain a multifilament; And treating the resulting multifilament with water and drying, followed by treatment with a finishing agent, wherein the finishing agent comprises polyether, a conjugated polyester having a molecular weight of 7,000 to 15,000 and a polybutene having a molecular weight of 4,000 to 8,000 And at least one selected from the group consisting of the polyketones. |
priorityDate | 2010-12-23^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |