http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20090078934-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_62bb25ebb7861ed6096674f0f61e9c8b
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2711-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2309-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2101-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B17-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-0001
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B7-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-00
filingDate 2008-01-16^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac166deb52bb31fc5ba5aa0bb3a9f299
publicationDate 2009-07-21^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20090078934-A
titleOfInvention Manufacturing method of recycled products using waste materials
abstract Disclosed is a method for producing renewable recycled materials using waste materials such as waste vinyl and paper sludge. In the present invention, 50 to 70% by weight of waste vinyl shredded with shredded vinyl is shredded, 30 to 50% by weight of ceramic powder or paper sludge ground to 200 mesh or less is mixed, and then a small amount of pigment is added to the mixture. Then, it is put into the injection machine of 300 ~ 500 degrees to manufacture recycled products.
priorityDate 2008-01-16^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458393356
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635

Showing number of triples: 1 to 21 of 21.