abstract |
Thermoplastic molding compositions, comprising A) from 10 to 99.999% by weight of a polyimide B) from 0.001 to 20% by weight of iron powder with a particle size of at most 10 μm (d50 value), which is obtainable via thermal decomposition of pentacarbonyliron, C) from 0 to 70% by weight of further additives, where the total of the percentages by weight of components A) to C) is 100%. |