Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dd2defce441ac6b2fe471dc39a39be50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73d55b44219a84c850812a4488def924 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L45-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 |
filingDate |
2009-06-22^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_918abf2808f3dafc865933f9e7b3146e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96453ae62e809bf624901439b17e64e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_987f77e776d3a0aeba6b4d2e7cde7b91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c94cfbf6a2c6a15130c45af047e9e55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f51d5e4dbba0b222f94fcebd3400d7a8 |
publicationDate |
2010-02-01^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201005025-A |
titleOfInvention |
B-pinene polymer composition and molded object obtained by using the same |
abstract |
Disclosed are: a polymer composition from which is obtained a molded body that has high heat resistance, low water absorbency, a low specific gravity, and excellent shock resistance; and a molded object which uses the polymer composition. The polymer composition is manufactured by combining a) a b-pinene polymer having a specific gravity of 0.85 or higher but less than 1.0 and a glass transition temperature of 80 DEG C or higher and b) an aromatic series vinyl block copolymer that comprises 10-35 mass% of an aromatic series vinyl polymer block and 65-90 mass% of a hydrogenated conjugate diene polymer block and that has a weight-average molecular weight of 100,000-250,000, these being combined such that the component a) is 60-95 parts by mass and the component b) is 5-40 parts by mass, with the total amount of component a) and component b) being 100 parts by mass. |