abstract |
The present invention provides a spherical powder aggregate comprising microcrystalline cellulose and a binder, and the powder agglomerate has a particle diameter of 1.0 to 6.0 mm, a breaking strength of 1.5 to 5.0 N, and a strain rate of 5.0 to 15.0%, and a production thereof. method. |