abstract |
The present invention provides an adhesive composition for a laminated laminate, a method for producing the same, a laminated body using the adhesive using the adhesive composition, and a secondary battery, wherein the adhesive composition for the laminated laminate and the laminated body The metal layer and the plastic layer are excellent in adhesion, and have electrolyte resistance even at low temperature curing. Its retention rate is high, and no interlayer peeling will occur over time.n n n An adhesive composition for lamination, which is an adhesive composition for lamination including a modified polyolefin resin (A), an amorphous polyolefin resin (B), and a hardener (C), wherein the amorphous polyolefin The content of the resin (B) is 0.1 mass% or more and less than 20 mass% with respect to the total mass of the solid content of the modified polyolefin resin (A) and the amorphous polyolefin resin (B). |