abstract |
Provided is a method for producing solutions, by which two solutions, namely a high-purity nickel sulfate solution and a mixed solution of nickel sulfate and cobalt sulfate are able to be obtained at the same time from a sulfuric acid solution containing nickel, cobalt and calcium. A method for producing solutions according to the present invention uses a sulfuric acid solution containing nickel, cobalt and calcium and performs a first step S 1 for producing a mixed solution of nickel sulfate and cobalt sulfate from the sulfuric acid solution and a second step S 2 for producing a solution of nickel sulfate from the sulfuric acid solution in parallel. In the first step, the sulfuric acid solution is subjected to solvent extraction by an extractant, thereby obtaining a first organic solvent after extraction. In the second step, the sulfuric acid solution is subjected to solvent extraction by means of an extractant. |