Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fcc0b66123940d1b32783569ebfa2d45 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16L11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-30 |
filingDate |
2007-12-28^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e3796660e46808ca4a1a66dab62db3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_927542615b9724b54c4e1477cd1e3110 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fefef5479804a742d7732c1bc70a0f2f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff7c1159aa7fcbea11ea1dd8a8f87e26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41ed9ee850fc8a0a18e38711dbcc6aee |
publicationDate |
2010-02-25^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2010048803-A1 |
titleOfInvention |
Method for producing polymer for oil-resistant rubber, polymer for oil-resistant rubber, composition for oil-resistant weather-resistant rubber, and rubber molded body |
abstract |
A method for producing a polymer for oil-resistant rubber, which comprises adding, to an aqueous dispersion of an unsaturated nitrile-conjugated diene copolymer (component A), a monomer composition (component B) containing at least one kind of monomer selected from the group consisting of a nitrile group-containing monomer (component B-1), a (meth)acrylic acid ester monomer (component B-2) and an aromatic vinyl compound monomer (component B-3), and conducting a polymerization reaction in a state that the ratio of the conjugated diene monomer present in the system, to the total monomers present in the system is controlled at 10 mol % or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016251454-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9293961-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10544234-B2 |
priorityDate |
2006-12-28^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |