abstract |
The present invention relates to a process for the production of polypropylene fibers and polypropylene spunbond nonwoven comprising a degradation step, wherein the melt flow of the polypropylene is increased, and a fiber or filament extrusion step. The present invention also relates to the fibers and nonwoven produced with said process and to composites and laminates comprising said fibers and nonwoven. |