Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2bc2da4bfebe79540ef2f4dac5deb0b4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-44 |
filingDate |
2006-05-09^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_326758c653b2ebe99dbdfe087fe54670 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab958217c43cbf19e08dec6b0a438990 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0578ff133393d294c954bc3ad700b2d7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0f0cdfaf454e7459cfa6f2cf9fee88e |
publicationDate |
2011-04-28^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011098423-A1 |
titleOfInvention |
Propylene-ethylene copolymers and process for their preparation |
abstract |
Random propylene/ethylene copolymers are provided characterized byn Ethylene content in the range of 4.5-7% wt; Mw/Mn (via GPC) in the range 3.5-5.5; Mz/Mw (via GPC) lower than 4; absence of 2-1 regioinversion, and Melting Temperature (Tm) (non-nucleated grade) lower than 143° C. nn The said copolymers show an excellent balance of impact and optical properties which is retained even after visbreaking. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015191852-A1 |
priorityDate |
2005-05-12^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |