abstract |
Provided is a process for producing an organic EL panel by using an ultrathin glass plate, in which the ultrathin glass plate is not “fractured” or “cut” in the production process, the organic EL element is formed reliably when formed by vacuum deposition, and recovered without damage after the production process, and there is no need for installing an additional step of cleaning the rear face of the ultrathin glass plate. The process for producing an organic EL panel according to the present invention is a process for producing an organic electroluminescent panel by forming an organic electroluminescent element on an ultrathin glass plate by vacuum deposition method, comprising forming electrodes on the ultrathin glass plate, by temporarily fixing the ultrathin glass plate to a supporting plate via a double-sided adhesive tape having a thermal release adhesive layer formed at least on one face of the base material layer, containing heat-expandable microspheres that start expansion and/or foaming at temperature higher than the vacuum deposition temperature. |