Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_41ac7ff6ab574ca3737b892da2ebfe6f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0411 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0435 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-661 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1397 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 |
filingDate |
2015-11-19^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd46e293650accc170d878b780f1bf28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_173e447bc23b4e69b318d133ea080063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f79e0a39be580d8b4f78c66d578d4f15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e012beb7f3d789c8176c8c039279d17 |
publicationDate |
2016-06-02^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2016156016-A1 |
titleOfInvention |
Method of manufacturing positive electrode for lithium ion secondary battery |
abstract |
A method of manufacturing a positive electrode includes: preparing a current collector foil having a first main surface and a second main surface; obtaining a granulated body in which a solvent remains by mixing a positive electrode active material, a conductive material, a binder, and the solvent with each other to obtain a mixture and granulating the mixture; obtaining a first positive electrode mixture layer by pressing the granulated body into a sheet shape; arranging the first positive electrode mixture layer on the first main surface; and heating the current collector foil in a state where the first positive electrode mixture layer is arranged on the first main surface, such that a temperature of the current collector foil becomes a softening point of the current collector foil or higher and that a temperature of the first positive electrode mixture layer is lower than a melting point of the binder. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10566610-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113394407-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018277832-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11223068-B2 |
priorityDate |
2014-11-27^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |