http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017190147-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_45251f99cd32300fd0ab35d04f692659
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2264-102
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-285
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2262-101
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-0062
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2607-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-145
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04B1-942
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B13-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B13-08
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B13-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B13-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04B1-94
filingDate 2015-12-31^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c6679661e5f3f6d0d64f5702451b326a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22db3091513513695e31aff3a2cfcaef
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb570fb711a366ccbdf50cc38025a8b2
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aace2ef39ac71ecca87eb6e16be0c049
publicationDate 2017-07-06^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2017190147-A1
titleOfInvention Fire Resistant Building Boards with Increased Amounts of Anti-Shrinkage Additives and Decreased Densities
abstract Disclosed is a building board with increased heat and fire resistance. Boards constructed in accordance with this disclosure have lower densities while at the same time containing larger amounts of anti-shrinkage materials. In one embodiment, a board was constructed with a density of less than 1,750 lbs/msf while at the same time including anti-shrinkage additives in amounts greater than 14% by weight of the core material. The inventors have discovered that beneficial, and heretofore unexpected, levels of fire resistance can be achieved by using increased amounts of anti-shrinkage additives in lower density building boards.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11034621-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10604929-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019068084-A3
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11339572-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11136757-B2
priorityDate 2015-12-31^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015125683-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017096369-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6643991-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-3689611-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3440
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419533897

Showing number of triples: 1 to 38 of 38.