abstract |
The present invention relates to a method to fill out uneven surfaces, whereby a fine grain, fusible powder is excessively applied to the surface to be treated, the excess is removed, and the remaining powder which fills cracks and cavities is temporarily heated to melt. The invention further reveals a means to carry out the method. |