abstract |
Substantially spherical mono-sized particles of zirconia can be prepared by the forced hydrolysis of an aqueous solution of zirconyl chloride. A zirconyl chloride solution having a molarity up to about 0.4 is heated for at least 72 hours at a temperature of at least 95° C. to generate suspended particles of hydrated zirconium oxide, which are recovered and calcined to provide the mono-sized zirconia powders. In preferred embodiments, mono-sized powders of a mixture of zirconia with one or more of its stabilizing metal oxides is prepared by precipitating the metal in the form of its hydroxide onto pre-formed zirconium-containing particles. |