abstract |
Heat-sealable, at least monoaxially orientated multi-layer film of a base layer of a polypropylene and at least one heat-sealable layer of 1. 35 to 70% by weight, preferably 38 to 60% by weight, of olefin polymers of (A) at least one terpolymer consisting of (a) 65 to 82% by weight of propylene, (b) 25 to 14% by weight of butene-1, (c) 10 to 4% by weight of ethylene, and (B) 0 to 7% by weight of a copolymer of ethylene and butene-1, wherein the sum of (A) and (B) or of (a) to (c) must always give 100% by weight and the monomer content of components (A) and (B) must always give 65 to 82% by weight of propylene, 25 to 14% by weight of butene-1 and 10 to 4% by weight of ethylene, 2. 65 to 30% by weight, preferably 62 to 40% by weight, of a propylene/ethylene copolymer with 2 to 6% by weight of ethylene, wherein the sum of 1. and 2. must always give 100% by weight, and 3. if appropriate customary auxiliaries and additives. |